چکیده: In this paper, an experimental investigation on the fatigue crack growth
behavior and the fatigue life of Modified Coach Peel -MCP- specimens are
carried out. The MCP specimens with 1 and 1.5 mm thickness and from
milled steel are used. The specimens are tested by a 25 kN capacity
INSTRON 8802 servo-hydraulic fatigue test machine under the various level
loadings with constant amplitudes. During the loading, the crack length and
the cycle numbers are measured accurately. The initiation and the
propagation of the spot weld specimens are approximately determined by
plotting the vertical position of the specimen versus the cycle’s curve. The
results show that, the initiation and the propagation of the cracks often
occurred for thinner plates. The results also indicate that the crack\\\\\\'s length
for thinner specimens is longer than that of the thicker specimens. It is also
found that the crack growth gradually in low level loadings while it is
usually growth around the nugget and eventually pull out the nugget for high
level loadings.
behavior and the fatigue life of Modified Coach Peel -MCP- specimens are
carried out. The MCP specimens with 1 and 1.5 mm thickness and from
milled steel are used. The specimens are tested by a 25 kN capacity
INSTRON 8802 servo-hydraulic fatigue test machine under the various level
loadings with constant amplitudes. During the loading, the crack length and
the cycle numbers are measured accurately. The initiation and the
propagation of the spot weld specimens are approximately determined by
plotting the vertical position of the specimen versus the cycle’s curve. The
results show that, the initiation and the propagation of the cracks often
occurred for thinner plates. The results also indicate that the crack\\\\\\'s length
for thinner specimens is longer than that of the thicker specimens. It is also
found that the crack growth gradually in low level loadings while it is
usually growth around the nugget and eventually pull out the nugget for high
level loadings.
کلیدواژه(گان): Fatigue Life of Modified Coach Peel,Spot Weld Specimens,
Fatigue Crack
کالکشن
:
-
آمار بازدید
An Experimental Investigation of Initiation, Propagation and the Fatigue Life of Modified Coach Peel -MCP- Spot Weld Specimens
Show full item record
contributor author | محمود شریعتی | en |
contributor author | محمد جواد مغربی | en |
contributor author | Mahmoud Shariati | fa |
contributor author | Mohammad Javad Maghrebi | fa |
date accessioned | 2020-06-06T13:44:43Z | |
date available | 2020-06-06T13:44:43Z | |
date issued | 2007 | |
identifier uri | https://libsearch.um.ac.ir:443/fum/handle/fum/3367356 | |
description abstract | In this paper, an experimental investigation on the fatigue crack growth behavior and the fatigue life of Modified Coach Peel -MCP- specimens are carried out. The MCP specimens with 1 and 1.5 mm thickness and from milled steel are used. The specimens are tested by a 25 kN capacity INSTRON 8802 servo-hydraulic fatigue test machine under the various level loadings with constant amplitudes. During the loading, the crack length and the cycle numbers are measured accurately. The initiation and the propagation of the spot weld specimens are approximately determined by plotting the vertical position of the specimen versus the cycle’s curve. The results show that, the initiation and the propagation of the cracks often occurred for thinner plates. The results also indicate that the crack\\\\\\'s length for thinner specimens is longer than that of the thicker specimens. It is also found that the crack growth gradually in low level loadings while it is usually growth around the nugget and eventually pull out the nugget for high level loadings. | en |
language | English | |
title | An Experimental Investigation of Initiation, Propagation and the Fatigue Life of Modified Coach Peel -MCP- Spot Weld Specimens | en |
type | Journal Paper | |
contenttype | External Fulltext | |
subject keywords | Fatigue Life of Modified Coach Peel | en |
subject keywords | Spot Weld Specimens | en |
subject keywords | Fatigue Crack | en |
journal title | International Journal of Applied Engineering Research | en |
journal title | International Journal of Applied Engineering Research | fa |
pages | 637-657 | |
journal volume | 2 | |
journal issue | 4 | |
identifier link | https://profdoc.um.ac.ir/paper-abstract-1073629.html | |
identifier articleid | 1073629 |