Synthesis and Microstructurral Study of Stereoblock Elastomeric Polypropylenes from Metallocene Catalyst (2-PhInd)2ZrCl2 Activated with Cocatalyst Mixtures
نویسنده:
, , , , , , ,سال
: 2013
چکیده: Various elastomeric polypropylenes (PPs) are synthe-
sized through homogeneous propylene polymerization with met-
allocene catalyst (2-PhInd)2ZrCl2 in the presence of different
cocatalyst mixtures: triethylaluminum (TEA)/methylaluminoxane
(MAO) or triisobutylaluminum (TIBA)/MAO in the range of AlAlR3/
AlMAO ¼ 0.0–0.9. The cocatalyst formulation impacts the resultant
polymer microstructure and the thermal and dynamic mechanical
properties of the produced PPs.
13
C NMR analysis of the polymers
reveals essentially atactic PP, with mmmm ¼ 7.9%, when AlAlR3/
AlMAO ¼ 0.0. The mmmm pentad content is maximized when
AlAlR3/AlMAO ¼ 0.8; for TIBA, mmmm ¼ 23.5%; and for TEA,
mmmm ¼ 17.6%. Differential scanning calorimetry analysis and
dynamic mechanical thermal analysis corroborate these findings.
Specifically, Tm, DHm,and Tg are essentially maximized under
these conditions, and the minimum damping is observed for
AlAlR3/AlMAO ¼ 0.6–0.8.
1
H NMR analysis of themixtures of catalyst
and cocatalysts (without monomer) shows very minor differences
for [Zr]:AlAlR3 in the range of 1:1–1:5.V C 2012Wiley Periodicals, Inc.
J. Polym. Sci., Part A: Polym. Chem. 2013, 51,724–731
sized through homogeneous propylene polymerization with met-
allocene catalyst (2-PhInd)2ZrCl2 in the presence of different
cocatalyst mixtures: triethylaluminum (TEA)/methylaluminoxane
(MAO) or triisobutylaluminum (TIBA)/MAO in the range of AlAlR3/
AlMAO ¼ 0.0–0.9. The cocatalyst formulation impacts the resultant
polymer microstructure and the thermal and dynamic mechanical
properties of the produced PPs.
13
C NMR analysis of the polymers
reveals essentially atactic PP, with mmmm ¼ 7.9%, when AlAlR3/
AlMAO ¼ 0.0. The mmmm pentad content is maximized when
AlAlR3/AlMAO ¼ 0.8; for TIBA, mmmm ¼ 23.5%; and for TEA,
mmmm ¼ 17.6%. Differential scanning calorimetry analysis and
dynamic mechanical thermal analysis corroborate these findings.
Specifically, Tm, DHm,and Tg are essentially maximized under
these conditions, and the minimum damping is observed for
AlAlR3/AlMAO ¼ 0.6–0.8.
1
H NMR analysis of themixtures of catalyst
and cocatalysts (without monomer) shows very minor differences
for [Zr]:AlAlR3 in the range of 1:1–1:5.V C 2012Wiley Periodicals, Inc.
J. Polym. Sci., Part A: Polym. Chem. 2013, 51,724–731
کلیدواژه(گان): catalysts,elastomers,metallocene catalysts,polyolefins,poly(propylene) (PP)
کالکشن
:
-
آمار بازدید
Synthesis and Microstructurral Study of Stereoblock Elastomeric Polypropylenes from Metallocene Catalyst (2-PhInd)2ZrCl2 Activated with Cocatalyst Mixtures
Show full item record
contributor author | G. H. Nejabat | en |
contributor author | M. Nekoomanesh | en |
contributor author | H. Arabi | en |
contributor author | H. Salehi-Mobarakeh | en |
contributor author | غلامحسین ظهوری | en |
contributor author | M. Omidvar | en |
contributor author | S. A. Miller | en |
contributor author | Gholamhossein Zohuri | fa |
date accessioned | 2020-06-06T13:11:27Z | |
date available | 2020-06-06T13:11:27Z | |
date issued | 2013 | |
identifier uri | http://libsearch.um.ac.ir:80/fum/handle/fum/3345234 | |
description abstract | Various elastomeric polypropylenes (PPs) are synthe- sized through homogeneous propylene polymerization with met- allocene catalyst (2-PhInd)2ZrCl2 in the presence of different cocatalyst mixtures: triethylaluminum (TEA)/methylaluminoxane (MAO) or triisobutylaluminum (TIBA)/MAO in the range of AlAlR3/ AlMAO ¼ 0.0–0.9. The cocatalyst formulation impacts the resultant polymer microstructure and the thermal and dynamic mechanical properties of the produced PPs. 13 C NMR analysis of the polymers reveals essentially atactic PP, with mmmm ¼ 7.9%, when AlAlR3/ AlMAO ¼ 0.0. The mmmm pentad content is maximized when AlAlR3/AlMAO ¼ 0.8; for TIBA, mmmm ¼ 23.5%; and for TEA, mmmm ¼ 17.6%. Differential scanning calorimetry analysis and dynamic mechanical thermal analysis corroborate these findings. Specifically, Tm, DHm,and Tg are essentially maximized under these conditions, and the minimum damping is observed for AlAlR3/AlMAO ¼ 0.6–0.8. 1 H NMR analysis of themixtures of catalyst and cocatalysts (without monomer) shows very minor differences for [Zr]:AlAlR3 in the range of 1:1–1:5.V C 2012Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013, 51,724–731 | en |
language | English | |
title | Synthesis and Microstructurral Study of Stereoblock Elastomeric Polypropylenes from Metallocene Catalyst (2-PhInd)2ZrCl2 Activated with Cocatalyst Mixtures | en |
type | Journal Paper | |
contenttype | External Fulltext | |
subject keywords | catalysts | en |
subject keywords | elastomers | en |
subject keywords | metallocene catalysts | en |
subject keywords | polyolefins | en |
subject keywords | poly(propylene) (PP) | en |
journal title | Journal of Polymer Science, Part A: Polymer Chemistry | fa |
pages | 724-731 | |
journal volume | 51 | |
journal issue | 51 | |
identifier link | https://profdoc.um.ac.ir/paper-abstract-1032609.html | |
identifier articleid | 1032609 |